Nov 13, 2022 at 6:35 | comment | added | P2000 | I think you meant to write that the patches of topping compound didn't bond to the paper tape? Both taping and topping mud are drying compounds and will shrink. It's hot mud that's a setting/curing compound and won't shrink. Topping compound cannot be used for the taping stage, which still supports your theory. | |
Nov 12, 2022 at 23:12 | comment | added | Mazura | Either they totally sucked at it or they embedded the tape with Plus X instead of Easy Sand, +1. If under the tape is water soluble, that's what they did. | |
S Nov 12, 2022 at 20:45 | review | First answers | |||
Nov 13, 2022 at 6:29 | |||||
S Nov 12, 2022 at 20:45 | history | answered | Keith Gordon | CC BY-SA 4.0 |